HPW designation:

HPW-202Cu

Abbreviation DIN EN 1044:

CU 202

DIN 8513

CuSn12

DIN EN ISO 17672

Cu 925

EN ISO 3677: 1995

B-Cu86Sn(P)-825/990

Composition (mass fraction in%):

Cu 86,6 - 88,9% | Sn 11,0 - 13,0% | P 0,01 - 0,4%

Working temperature ° C:

11040 °C

Temperature ° C:

Solidus 825 °C, Liquidus 990 °C

Tensile strength of the soldering [N/mm²]

k.A.

Density[g/cm³] :

8,6

Application

Steel, nickel and nickel alloys, chrome and chrome-nickel-steel, gas-shielded brazing, vacuum brazing.