HPW designation:

HPW-101Cp

Abbreviation DIN EN 1044:

CP 101

DIN 8513

-

DIN EN ISO 17672

CuP 286

EN ISO 3677: 1995

B-Cu75AgP-645

Composition (mass fraction in%):

Cu 73,5 - 76,4% | Ag 17,0 - 19,0% | P 6,6 -7,5%

Working temperature ° C:

0650 °C

Temperature ° C:

Solidus 645 °C, Liquidus 645 °C

Tensile strength of the soldering [N/mm²]

250

Density[g/cm³] :

8,4

Application:

Copper on copper without flux, red brass, brass and copper-tin-alloys with flux. Not to use with sulfate media, iron- and nickel alloys, heat-resisting up to 200°C