HPW designation:

HPW-201Cu

Abbreviation DIN EN 1044:

CU 201

DIN 8513

CuSn6

DIN EN ISO 17672

Cu 922

EN ISO 3677: 1995

B-Cu94Sn(P)-910/1040

Composition (mass fraction in%):

Cu 92,6 - 94,5% | Sn 5,5 - 7,0% | P 0,01 - 0,4%

Working temperature ° C:

11060 °C

Temperature ° C:

Solidus 910 °C, Liquidus 1040 °C

Tensile strength of the soldering [N/mm²]

k.A.

Density[g/cm³] :

8,7

Application:

Steel, nickel and nickel alloys, chrome and chrome-nickel-steel, gas-shielded brazing, vacuum brazing.
+49 7232 80978-0 info@hpwirth.com +49 7232 80978-0 info@hpwirth.com