HPW descripton:

HPW-104Al

Abbreviation DIN EN 1044:

AL 104

DIN 8513

-

DIN EN ISO 17672

Al 112

EN ISO 3677:1995

B-Al88Si-575/585

Composition (Mass fraction in %):

Al 85,5 - 89,0% | Si11,0 - 13,0% | Fe 0 - 0,8% | Cu 0 - 0,3% | Zn 0 - 0,2% | Mn 0 - 0,15% | Mg 0 - 0,1%

Working temparature °C:

0590 °C

Temperature °C:

Solidus 575 °C, Liquidus 585 °C

Tensile strength of the join [N/mm²]

no information

Density [g/cm³]:

2,65

Applications

Aluminium